Products

We have different technology thru which the different grades are produced and major difference identified in rCB produced from both above technology is in tint strength and tensile values.

  • CC R Grade – Impact Classifier Micronizer
  • CC P Grade – Roller Attrition Micronizer
Quality ParametersUOMCC-RCC-PTesting Standard
Toluene Discoloration%transmittance>85>85ASTM D-1618
Sieve Residue:   
325 Meshppm<500<500ASTM D-1514
100 MeshppmNilNilASTM D-1514
35 MeshppmNilNilASTM D-1514
pH 6.75-7.756.75-7.75ASTM D-1512
Particle Size(d90)Micron<25<15
Moisture (Heat Loss)%<2<2ASTM D-1509
Ash #%<22<22ASTM D-1506
Sulphur Content%<4<4ASTM D-129
Physical Form Powder and PelletsPowder and Pellets
Pellet Hardnessgf<50<50ASTM D-3313
Fines%<10<10ASTM D-1508
Pour Density in PelletsKg/m3490-550490-550ASTM D-1513

#Ash content comprises of Silica, Zinc oxide, Calcium Carbonate and other filler material used while manufacturing of tyres